Konpozisyon chimik
Hastelloy C2000 8.0 * 1.25 mm mawonnen tib
Konpozisyon chimik Hastelloy C-2000 endike nan tablo ki anba a:
Eleman | % min | Max % |
---|---|---|
Cr | 22.00 | 24.00 |
Mo | 15.00 | 17.00 |
Fe | – | 3.00 |
C | – | 0.01 |
Si | – | 0.08 |
Co | – | 2.00 |
Mn | – | 0.50 |
P | – | 0.025 |
S | – | 0.01 |
Cu | 1.30 | 1.90 |
Al | – | 0.50 |
Ni | bal |
Detay alyaj
Hastelloy C-2000 dansite, pwen k ap fonn, koyefisyan ekspansyon, ak modil elastisite endike nan tablo ki anba a:
Dansite | Pwen k ap fonn | Koefisyan ekspansyon | Modil Rigidite | Modil Elastisite |
---|---|---|---|---|
8.5 g / cm³ | 1399 °C | 12.4 μm/m °C (20 - 100 °C) | 79 kN/mm² | 206 kN/mm² |
0.307 lb/pous³ | 2550 °F | 6.9 x 10-6an/an °F (70 – 212 °F) | 11458 ksi | 29878 ksi |
Tretman chalè nan pati fini
Hastelloy C2000 8.0 * 1.25 mm mawonnen tib
Tretman chalè tipik Hastelloy C-2000:
Kondisyon jan AWI te founi | Kalite | Tanperati | Tan | Refwadisman |
---|---|---|---|---|
Tanperaman rkwit oswa Spring | Soulaje estrès | 400 - 450 °C (750 - 840 °F) | 2 Hr | Air |
Hastelloy C2000 8.0 * 1.25 mm mawonnen tib
Pwopriyete
Pwopriyete mekanik tipik Hastelloy C-2000:
Rkwit | ||
---|---|---|
Apeprè.fòs rupture | <1000 N/mm² | <145 ksi |
Apeprè.tanperati opere depann sou chaj** ak anviwònman an | -200 a +400 °C | -330 a +750 °F |
Hastelloy C2000 8.0 * 1.25 mm mawonnen tib
Tanperaman prentan | ||
---|---|---|
Apeprè.fòs rupture | 1300 - 1600 N/mm² | 189 – 232 ksi |
Apeprè.tanperati opere depann sou chaj** ak anviwònman an | -200 a +400 °C | -330 a +750 °F |