KONPOZISYON CHIMIK
incoloy 625 tubing bobin tib kapilè
C | Cr | Ni | Fe | Mn | Si | Mo | Co | P | S | Ti | Nb + Ta | Al |
---|---|---|---|---|---|---|---|---|---|---|---|---|
≤ 0.1 | 20-23 | ≥ 58 | ≤ 5 | ≤ 0.5 | ≤ 0.5 | 8-10 | ≤ 1* | ≤ 0.015 | ≤ 0.015 | ≤ 0.4 | 3.15 - 4.15 | ≤ 0.4 |
(mas %)
*Si yo detèmine
ASTM B444, ASME SB444, AMS 5581
Dapre ASTM B444, ASME SB444, AMS 5581
Kondisyon | Fòs rupture | Sede fòs | Elongasyon |
minimòm, ksi | minimòm, ksi | minimòm, % | |
Klas 1 | 120 | 60 | 30 |
Klas 2 | 100 | 40 | 30 |
* Pi wo pwopriyete fòs yo ka bay nan kondisyon an frèt fè tèt di.
incoloy 625 tubing bobin tib kapilè
70°F | 200°F | 400°F | 600°F | 800°F | 1000°F | ||
---|---|---|---|---|---|---|---|
Dansite | liv/pous3 | 0.305 | - | - | - | - | - |
Ekspansyon tèmik | X10-6/°F | - | 7.1 | 7.3 | 7.4 | 7.6 | 7.7 |
Modil elastik | 103 ksi | 30.1 | 29.6 | 28.7 | 27.8 | 26.9 | 25.7 |
Poisson rapò | - | 0.278 | 0.28 | 0.286 | 0.29 | 0.295 | - |
Kondiktivite tèmik | Btu-an/h·ft2·°F | 68 | 75 | 87 | 98 | 109 | 139 |
Espesifik Chalè | Btu/lb·°F | 0.098 | 0.102 | 0.109 | 0.115 | 0.122 | 0.118 |
Sede fòs | ksi | 70 | 68 | 63 | 60 | 59 | 34 |
Fòs rupture | ksi | 140 | 134 | 130 | 129 | 129 | 88 |
incoloy 625 tubing bobin tib kapilè
PWOSESISDESCRIPTIONSsteel MakingElectric Arc Furnace ki te swiv pa Vacuum Oxygen Decarburization (VOD) oswa Argon Oxygen Decarburization (AOD).Pipe MakingConventional Seamless Frèt Fini tiyo ak Tib Faktori Pwosesis.Heat TreatmentCannot dwe fè tèt di pa tretman chalè.Yo ka bay nan kondisyon an annealed, solisyon annealed oswa frèt fè tèt di.Kondisyon an rkwit fòs ki pi wo a anjeneral travay nan sèvis jiska 1100 ° F, pandan y ap kondisyon an rkwit solisyon yo itilize nan aplikasyon pou pi wo a 1100 ° F.